Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Thermogravimetric Analysis (TGA) Loss on Drying Testing: Principles, Standards, and Applications

Thermogravimetric analysis (TGA) loss on drying testing is a high-precision technique that measures the mass loss of a sample as it is heated under a controlled atmosphere, quantifying moisture, residual solvents, and other volatile components within minutes. It is widely applied to polymers, pharmaceuticals, foods, chemicals, and advanced materials for quality control, incoming material inspection, and research and development. This article explains the working principle, applicable standards, sample requirements, testing procedures, and typical applications of TGA-based loss on drying experiments.

Technical Overview

Thermogravimetric analysis (TGA) is an analytical technique that continuously records the mass of a specimen as a function of temperature or time while the specimen is subjected to a precisely controlled temperature program and purge atmosphere. A thermobalance consists of a sensitive microbalance, typically with a resolution of 0.1 to 1 microgram, a programmable furnace, a sample pan made of alumina or platinum, and a gas flow system supplying inert nitrogen or oxidative air and oxygen atmospheres.

In a loss on drying (LOD) experiment by TGA, the sample is heated from ambient temperature to a specified drying temperature, or held isothermally at that temperature, and the percentage of mass lost is recorded. This mass loss corresponds to the release of surface moisture, bound water, residual solvents, and other volatile substances. The resulting thermogravimetric (TG) curve and its derivative (DTG curve) allow overlapping mass-loss events to be separated by their characteristic temperature ranges, which is a decisive advantage over conventional oven-drying methods.

Compared with traditional oven or halogen moisture balance procedures, TGA loss on drying testing offers several benefits: it requires only milligram-scale samples, is fully automated, completes within 20 to 60 minutes, and simultaneously provides additional information such as decomposition onset temperature, volatile fraction, combustible content, and ash residue. These capabilities make TGA a powerful tool in accredited third-party laboratories as well as in industrial quality control and research environments.

Testing Samples

Polymers and Plastics

Thermoplastic resins, pellets, granules, films, and fibers, including polyethylene, polypropylene, PET, polyamide, polycarbonate, and ABS, are routinely tested for moisture before melt processing. Excessive moisture in hygroscopic polymers such as PET and polyamide can cause hydrolytic degradation, silver streaks, and bubbles during injection molding or extrusion.

Pharmaceutical and Nutraceutical Materials

Active pharmaceutical ingredients (APIs), excipients, granules, lyophilized powders, and plant extracts are tested for water content and residual solvents, which directly affect flowability, compaction behavior, chemical stability, and shelf life.

Food and Agricultural Products

Milk powder, starches, flours, proteins, spices, tea, and other food ingredients are evaluated for moisture content, which influences nutritional labeling, processing behavior, microbial stability, and storage performance.

Chemicals, Coatings, and Fine Powders

Pigments, dyes, fillers such as calcium carbonate and talc, catalysts, adhesives, and coating powders are tested to verify drying specifications and volatile organic content.

Battery and Advanced Materials

Cathode and anode active materials, conductive carbons, binder powders, and electrolyte salts require strict moisture control, because trace water can trigger side reactions and degrade electrochemical performance and safety.

Inorganic, Mineral, and Rubber Materials

Ceramic powders, clays, ores, coal, coke, and elastomeric compounds can be characterized for moisture, volatile matter, and filler or carbon black content in a single TGA run.

Testing Items

Typical test items and deliverables for TGA loss on drying experiments include:

  • Moisture content and total loss on drying at a specified temperature, for example 105 °C
  • Volatile matter and residual solvent content released below a defined temperature threshold
  • Decomposition onset temperature and thermal stability assessment
  • Stepwise compositional analysis: moisture, volatiles, combustible organic fraction, and inorganic ash residue
  • Filler, glass fiber, or carbon black content in polymer and rubber compounds
  • Derivative (DTG) peak temperatures and maximum mass-loss rates for kinetic comparison
  • Residual mass (ash) after oxidative burn-off in air or oxygen atmosphere

Testing Methods

Sample Preparation

A representative specimen of typically 5 to 20 mg, or up to 50 mg for heterogeneous materials, is homogenized and loaded into an open alumina or platinum pan. Samples may be powders, pellets, films, fibers, or small sections cut from larger parts. Care is taken to minimize moisture exchange with ambient air between sampling and analysis.

Instrument Setup and Calibration

The microbalance is calibrated with certified mass standards, and the furnace temperature is calibrated using Curie-point or melting-point reference materials. High-purity nitrogen is supplied at a flow rate of 20 to 60 mL/min for inert drying and decomposition steps, while compressed air or oxygen is used for oxidative ash determination.

Typical Test Procedure

A common loss on drying program is as follows: equilibrate the sample at ambient temperature or 40 °C, heat at 10 °C/min to the specified drying temperature such as 105 °C, and hold isothermally until the mass change falls below a constant-mass criterion, for example less than 0.05% per 5 minutes. For full compositional analysis, the run continues under nitrogen to approximately 600 °C, after which the atmosphere is switched to air or oxygen and the temperature is raised to 800 to 900 °C to burn off carbon and quantify the inorganic ash residue.

Calculation of Results

Loss on drying is calculated as the percentage of mass lost relative to the initial sample mass: LOD (%) = (m0 − m1) / m0 × 100, where m0 is the initial mass and m1 is the mass at the specified endpoint. The DTG curve is used to confirm that the drying step is fully separated from any decomposition event, ensuring the validity of the result.

Reference Standards

  • ASTM E1868 — Standard Test Methods for Loss-On-Drying by Thermogravimetry
  • ASTM E1131 — Standard Test Method for Compositional Analysis by Thermogravimetry
  • ASTM D6370 — Standard Test Method for Rubber Compositional Analysis by Thermogravimetry (TGA)
  • ISO 11358 series — Plastics: Thermogravimetry (TG) of polymers
  • ISO 9924 series — Rubber and rubber products: Determination of composition by thermogravimetry
  • GB/T 6284 — Determination of loss on drying for chemical products
  • GB/T 27761 — General rules for thermogravimetric analysis

Applications

TGA loss on drying testing is applied across a broad range of industrial and scientific scenarios:

  • Incoming quality control of hygroscopic resins before injection molding and extrusion to prevent hydrolysis and surface defects
  • Moisture verification of battery electrode materials and electrolyte salts to ensure cell safety and performance
  • Pharmaceutical batch release testing, stability studies, and drying process validation
  • Food ingredient moisture determination for labeling compliance, shelf-life estimation, and process control
  • Verification of filler, fiber, and carbon black content in polymer compounds and rubber formulations
  • Research and development studies on thermal stability, degradation kinetics, and formulation comparison
  • Failure analysis of degraded or contaminated parts through characteristic mass-loss fingerprints
  • Support of regulatory submissions and customer specifications through testing at accredited third-party laboratories

FAQ

Question: How is TGA loss on drying different from oven drying or a halogen moisture balance?

TGA uses milligram-scale samples and a programmable temperature and atmosphere profile, completing a typical determination in 20 to 60 minutes. It also separates overlapping mass-loss steps and can extend the analysis to decomposition and ash content in the same run. Oven and halogen methods typically require gram-scale samples, fixed temperatures, and longer times, and cannot distinguish water from other volatiles.

Question: Does loss on drying equal water content?

Not necessarily. The TGA mass loss includes all substances volatilized below the specified endpoint, such as residual solvents and low-boiling additives, in addition to water. If a specific water value is required, Karl Fischer titration is recommended as a complementary method.

Question: How do I choose the drying temperature?

The temperature is defined by the relevant product specification or standard. A temperature of 105 °C is common for free water, while some materials require 120 to 130 °C or material-specific conditions. The chosen temperature must remain safely below the decomposition onset to avoid overestimating volatile content.

Question: What sample size and accuracy can be expected?

Typical specimen masses are 5 to 20 mg. With microbalance resolution at the sub-microgram level, mass losses on the order of 0.01% to 0.1% can be reliably detected, depending on sample size and homogeneity.

Question: What is reported in a TGA loss on drying test report?

A professional report includes the initial sample mass, the complete temperature program and atmosphere, the TG and DTG curves, the calculated loss on drying percentage, any additional stepwise mass losses, the residual or ash mass, and the applicable test standard. This documentation ensures traceability and supports comparison with specification limits.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time
  • Competitive pricing